1, when the brazing metal and solder contain toxic metal components to stringent protective measures, so that the operator poisoning
These metals include Be, Cd, Pd, Zn.
2, Be in atomic energy, aerospace and electronics industry application value is high, but it is toxic, Welding Wiresshould pay special attention to the safety of anti-
Protection measures. Be mainly inhaled through the respiratory tract and skin damage from the body slow speed, short-term inhalation of a large number of
Can cause acute poisoning, inhalation of BeO and other insoluble compounds can cause chronic poisoning, beryllium disease, a few years after the onset, mainly for the call
Respiratory tract lesions. Brazing of beryllium and beryllium oxide, preferably in a closed ventilation equipment, and should have purification devices to reach the required standard
Prospective only from the outdoors.
3, Cd is usually in order to improve Brazing Alloy process to join in the solder elements, volatile when heated, from the respiratory and digestive
Road inhalation, the savings in the kidney, intrahepatic, and more, and excreted in the bile, short-term inhalation of Cd dust or vapors can cause acute
Poisoning, long-term, low-concentration exposure to Cd smoke vapor, can cause emphysema, kidney damage, olfactory disorder and osteomalacia psychosis
.
4, Pb is the main component of the soft solder, heated to 400 ~ 500 ℃, can produce large amounts of Pb vapor in the air quickly
Generate lead oxide, Pb and its compounds have similar toxicity, mainly in the form of soot vapor to enter the body through the respiratory tract when brazing
Can also be absorbed through the skin wound.
Pb vapor poisoning is usually chronic poisoning, mainly as neurasthenic syndrome, digestive disorders, anemia, peripheral
Neuritis, kidney, liver and other organ damage. Current provisions of the air of workplace maximum allowable concentration of lead smoke 0.03mg/m3
The lead dust 0.05mg/m3.
6, Zn and its compounds ZnCl2 brazing, volatile Zn and ZnCl2 will generate zinc smoke inhaled can cause metal fume fever
(Metal fume fever), symptoms are trembling, fever, sweating, nausea, headache, limb weakness. Exposure to ZnCl2 smoke
Mist may cause lung damage, contact with ZnCl2 solution may cause skin ulcers. Therefore, to prevent smoke exposure to the human body, must be applied to individual
Protective equipment and good ventilation, when the skin is touched ZnCl2 solution requires a lot of water to flush the affected area.
7, the use of fluoride-containing flux must be well ventilated conditions brazing, or use of personal protective equipment
. When the fluoride flux dip brazing, the exhaust system must ensure that the environmental concentrations within the provisions of the existing national
Specify a maximum allowable concentration for 1mg/m3.
8, the dangers of fluoride on the human body is mainly manifested as bone pain, osteoporosis, or deformation, severe cases spontaneous fractures
. The damage to the skin, itching, pain, and eczema.
To clean metal parts before brazing, the use of cleaning agents, including organic solvents, acids and alkalis and other chemicals
Toxic vapor would evaporate during the cleaning process, requiring a well-ventilated and meet the state requirements to ensure the safety of the operator's
Whole.
Dip brazing is divided into the salt bath brazing and metal bath Brazing Alloy. They are brazed parts locally or totally immersed in molten salt solution or
The molten solder heating and brazing methods. Baptist Put brazing heating speed, high production efficiency, liquid media
The shielded arc welding is not oxidized. Especially suitable for large-scale continuous production. The disadvantage is that the energy consumed in large quantities, brazing process from the molten salt
Volatile large amounts of harmful gases, serious environmental pollution. Dip brazing the personal safety of the welding operation.
Used in the salt bath brazing salts containing chloride, fluoride and cyanide, and it show in the heating process in Welding ElectrodesSeriously volatile toxic gases. In addition, the solder containing volatile metals such as zinc, tin, lead, hinge, these metals
Such as hinge steam even toxic vapors harm the human body 10. Soldering, brazing flux contained in the organic solution steamed refund issued
To the gas on the human body is also very harmful to the mouth therefore,
The case of steam, we must take effective ventilation measures to exclude.
In addition, in the dip brazing process, it is particularly important should be immersed in the salt bath tank: weldment must be baked very
Dry, water shall not be left in the weldment, or when immersed in salt bath tank, and instantly you can generate a lot of steam, so that the solution to splash
Dramatic explosion, caused by strict: the fire and burn the body, flux is added to the salt bath tank must also be prior to the
The solder engine agent is fully dry, not only requires, inter